Just test with a magnet
On Aug 3, 2010 12:59 PM, "Dick Wampach" <rwampach@att.net> wrote:
Rob, I doubt that any manufacture would make a f/w that was not to
standards for heat resistance.
You could try to test the material with a file, if an edge is accessible in
a non critical location. Alum is soft, SS is much harder, you should be
able to tell the difference with just a few strokes.
Dick
-----Original Message-----
From: mike.davis@dcsol.com [mailto:mike.davis@dcsol.com] On Behalf Of...
schaumr@dcsol.com
Sent: Tuesday, August 03, 2010 9:53 AM
To: rebel-builders@dcsol.com
Subject: [rebel-builders] Firewall material for Reb #786 (manufactured
2003-2004)?
Hi All,
All th...
-----------------------------------------------------------------
List archives located at: https://mail.dcsol.com/login
username "rebel" password "builder"
Unsubs...
-----------------------------------------------------------------
List archives located at: https://mail.dcsol.com/login
username "rebel" password "builder"
Unsubscribe: rebel-builders-unsubscribe@dcsol.com
List administrator: mike.davis@dcsol.com
-----------------------------------------------------------------
Do you want this big green box to go away? Well here's how...
Click here for full update
Wildcat! photo archives restored.
Click here for full update
Donors can now disable ads.
Click here for instructions
Add yourself to the user map.
Click here for instructions
Click here for full update
Wildcat! photo archives restored.
Click here for full update
Donors can now disable ads.
Click here for instructions
Add yourself to the user map.
Click here for instructions